DEMARTIN chemical nickel

  • Corrosion protection
  • Wear protection
  • Exact edges in forming

 

Process variants

Chemical nickel High-Phos

 Standard coating with a phosphorous content of 9-12% by weight that is characterised by a high degree of corrosion protection and ductility; coating applicable to all common basic materials; glossy.

Chemical nickel Mid-Phos

 Special process with a phosphorous content of 5-9% by weight that is characterised by a high degree of hardness and gloss; coating applicable to all basic materials.

Chemical nickel – thermal post treatment

 Through thermal post treating, the surface hardness and wear behaviour of chemical nickel coatings can be increased. It has also been demonstrated that this post treatment process results in a better coating adhesion. We are able to perform this hardening under atmospheric conditions and under a protection gas.

specifications

Coating material

Ni/P

Process type

Autocatalytic

Colour

Metallic

Hardness [HV]

600/1000(tempered)

Application temperature [°C]

<600

Deposition temperature [°C]

<90

Density [g/cm3]

7.5-8.3

uses

industries
  • Medical technology
  • Machine industry
  • Semiconductors
  • Textile machine industry
  • Energy and electrical engineering
  • Mould and tool construction
  • Plant and apparatus construction
  • Arms industry
  • Automobile industry
Schichtdickenempfehlung

Loading type

Coating thickness

mild wear and tear,
mild corrosion stress

5 - 10 µm

medium wear and tear,
medium corrosion stress

10 - 25 µm

high wear and tear,
high corrosion stress

25 - 50 µm

very high wear and tear,
very high corrosion stress

> 50 µm